01

Ready-mixed concrete

The slump that matters is the one at the pump, not the one at the plant. Haul time, ambient temperature, and the cement's C₃A and alkali content all bend the retention curve, which is why the same admixture can behave well on one route and badly on the next.

  • Short haul, strength-driven mixes: CU-100 at the low end of its dosage range.
  • Drum time over an hour, or 30 °C and above: CU-200, or a 30:70 blend with CU-100.
  • Sand with a methylene blue value above 1.4 g/kg: CU-400 before raising the dose — extra polycarboxylate mostly feeds the clay.
  • Dosage set by trial on the cement and sand actually in the yard — not from a datasheet.
GradeCU-100 · CU-200 · CU-400 Dosage0.15–0.55 %
02

Precast and prestressed

Steel moulds show every defect. Blowholes, edge tearing and colour variation are the three complaints that come back from a precast line, and all three are controlled by air content and rheology rather than by water reduction alone.

  • Early demould strength from CU-300: the 12–24 h figure is what the mould cycle runs on.
  • Steam-cure stability at 60–80 °C; verify the demould strength against the cycle, not the 28-day figure.
  • If the surface is the problem — blowholes, edge tearing, colour — check air content and vibration before changing the admixture.
GradeCU-300 · CU-100 Dosage0.20–0.50 %
03

Self-compacting concrete

SCC fails in one of two ways: it blocks at the reinforcement, or it bleeds and segregates after placement. Both are rheology problems, and both are sensitive to the sand's fines content and to the viscosity-modifying agent in the mix.

  • Balance yield stress with a CU-100 / CU-200 blend and plastic viscosity with CU-500, rather than pushing one grade.
  • Low bleeding at high paste volume; check with the sieve segregation test, not by eye.
  • Fines-deficient sand may need a VMA — the PCE dosage alone will not fix segregation.
GradeCU-500 · CU-200 · CU-100 Dosage0.25–0.60 %
04

High-strength concrete

Above C60 the water/binder ratio drops below 0.30 and the mix becomes a paste problem. Dispersion has to work at dosages where adsorption sites on the cement are already saturated, and the silica fume or slag in the blend changes both the surface chemistry and the set time.

  • High grafting-density grades hold dispersion where adsorption sites are saturated.
  • CU-500 lowers plastic viscosity below w/b 0.30 — pump pressure falls before the dosage does.
  • Set time shifts with silica fume and slag — measure, then adjust with retarder, not with more PCE.
GradeCU-500 · CU-100 Dosage0.30–0.70 %
05

Mass, marine and underground

Three different problems that share one requirement: the mix has to still be the mix you designed, hours later and metres deep. Mass pours constrain heat, marine work constrains chloride, and sprayed concrete constrains how fast the mix can set on the wall.

  • Mass pours: retarder plus CU-200; keep the temperature differential inside the project's limit, and verify with the actual cement heat curve.
  • Marine and sulfate exposure: low-chloride PCE plus a binder designed for the exposure class; the admixture does not substitute for the binder.
  • Tunnel linings and water-retaining sections: CU-600 where the specification caps crack width — those mixes are governed by shrinkage, not by strength.
  • Shotcrete: a separate accelerator system — PCE sets the base mix workability, the accelerator sets the build-up.
GradeCU-200 · CU-100 · CU-600 Dosage0.20–0.55 %
06

Grout, mortar and repair

Small volumes, high surface-to-volume ratios, and a short window between mixing and placement. Bleeding is the failure mode that matters: a grout that bleeds leaves a plane of weakness exactly where the load is transferred.

  • Low-bleeding formulation for vertical and overhead repair.
  • Extended working time for hand-placed repair mortar without retarding the final set too far.
  • Chloride-free for repair in contact with reinforcement.
GradeCU-300 · CU-200 Dosage0.15–0.40 %

What a trial needs

Five things in, one dosage plan out

  • Cement analysis and strength report (C₃A, alkali, fineness)
  • SCM type and ratio: fly ash class, slag fineness, silica fume
  • Sand fineness modulus and methylene blue value; maximum aggregate size
  • Current mix design, with target slump at discharge and on arrival
  • Haul distance and time, and the ambient temperature on site

Request a sample →

What the trial measures

The raw sheet, not a summary

  • Paste flow and flow loss at 0, 30, 60, 120 min
  • Mortar water reduction to GB/T 8077 or equivalent
  • Concrete slump, spread, air content and setting time
  • Compressive strength ratio at 3, 7 and 28 days
  • Bleeding rate and slump change over one hour

The trial report ships with the sample. Where a third-party report is required, testing goes to a laboratory recognised in the destination country, quoted separately.